Looking for ASTM A924 Hot-Dip Coated Steel Coil?

ASTM A924

Definition

This specification covers the general requirements for steel sheets in coils and cut length, metallic-coated on continuous lines by the hot-dip process.

This material is intended for applications requiring corrosion resistance. Hot-dip metallic coatings are available in six different types: zinc and zinc-iron alloy, lead-tin alloy, aluminum, aluminum-zinc alloy, zinc-aluminum alloy, and zinc-aluminum-magnesium alloy

This specification covers the general requirements that, unless otherwise specified in the product specification, apply to steel sheet in coils and cut lengths, metallic-coated on continuous lines by the hot-dip process.

The product is intended for applications requiring corrosion resistance. The product specifications contain requirements for specific strength levels, heat resistance, paintability, or formability, or a combination thereof.

ASTM A924 PDF Free Download

ASTM-A924

Chemical Composition

TABLE 1 Product Analysis Tolerances
ElementLimited or Maximum of Specifified Element, %Tolerance
Under
Minimum
Limit
Over
Maximum
Limit
CarbonTo 0.15, incl 0.020.03
Over 0.15 to 0.40, incl0.030.04
Over 0.40 to 0.80, inc0.030.05
Manganese To 0.60, incl 0.030.03
Over 0.60 to 1.15, incl0.040.04
Over 1.15 to 1.65, incl 0.050.05
Phosphorus......0.01
Sulfur......0.01
SiliconTo 0.30, incl0.020.03
Over 0.30 to 0.600.050.05
Copper...0.02...
TitaniumTo 0.10, incl 0.01A0.01
VanadiumTo 0.10, incl 0.01A0.01
Over 0.10 to 0.25, incl0.020.02
ColumbiumMinimum only specifified0.01...
To 0.10, incl 0.01A0.01
"A"If the minimum of the range is 0.01 %, the under tolerance is 0.005 %.

The chemical composition requirements of the base steel are shown in the individual product specifications.

An analysis of each heat shall be made by the manufacturer to determine the percentage of carbon, manganese, phosphorus, sulfur, and any other elements specified or restricted by the individual product specification.

When desired, product analysis shall be made by the purchaser on the finished product. The product analysis so determined shall meet the tolerances shown in the table.

Capped or rimmed steels are not technologically suited to product analysis due to the nonuniform character of their chemical composition, and therefore, the tolerances in

Table 1 does not apply. Product analysis is appropriate on these steels only when misapplication is apparent.

Product analysis for phosphorus or sulfur is not technologically appropriate because of the segregation of these elements in non-skilled steels. Product analysis is appropriate only when misapplication is apparent.

Samples for product analysis shall be drillings through areas stripped free of coating. At least three pieces shall be selected, but if the product of more than one mill lift or coil is involved, at least six pieces shall be selected.

When supplying High-Strength Low-Alloy Steel (HSLA), some producers use one or more microalloying elements as strengthening agents or use alloy additions to effect inclusion control or both. The producer shall be consulted for the specific chemical composition applied. If any alloying addition is known to be of concern to the user, the producer shall be notified of this concern.

Method of Analysis—The determination of chemical composition is permitted to be made by any test method, except in case of dispute, where the referee test methods listed in the section on test methods of Test Methods A 751 shall be used.

Coating:

Coating Analysis—The nominal composition of the coating is described in the individual product specification.

Method of Analysis—The determination of chemical composition shall be made in accordance with acceptable chemical, spectrochemical, or other test methods.

Thickness Tolerance  ASTM A924

Thickness Tolerance  ASTM A924 (3/8 Inch Minimum Edge Distance)
Unit: Inch. Plus and minus for specified thickness (including base metal and coating)
Width/Thicknessthrough 0.023Over 0.023 through 0.043Over 0.043 through 0.061Over 0.061 through 0.075Over 0.075  through 0.101over 0.101 through 0.187
To 32 incl.0.0030.0040.0050.0060.0070.008
Over 32 to 40 incl.0.0030.0040.0050.0060.0080.008
Over 40 to 60 incl.0.0030.0040.0050.0060.0080.009
Over 60 72 incl.  -0.0040.0050.0060.0090.009

Length Tolerances ASTM A924

Length Tolerances ASTM A924
Unit: Inch. Tolerance over specified length. No minus tolerance.
LengthTolerance
Over 12 through 301/8
Over 30 through 601/4
Over 60 through 961/2
Over 96 through 1203/4
Over 120 through 1561
Over 156 through 1921.25
Over 192 through 2401.5
Over 2401.75

Width Tolerances ASTM A924

Width Tolerances ASTM A924
Unit: Inch. Tolerance over specified width. No minus tolerance
WidthTolerance
Over 12 through 301/8
Over 30 through 483/16
Over 48 through 601/4
Over 60 through 725/16
5/5 - (1 vote)
Facebook
Twitter
LinkedIn
Pinterest
Latest Posts

Related Posts

EN 10130

The specifications and delivery-related technical conditions for low carbon steel flat products that have been cold rolled are described in EN 10130 as approved by

Read More

ASTM A1008

If you’re looking for tough steel material, ASTM A1008 is standard-grade carbon steel. It is used in various construction applications, even in aerospace industries. What

Read More

EN 10025

The specifications for manufacturing steel products are laid out in an EN steel standard. Generally speaking, EN standards must be followed if you operate in

Read More